Open-access Temperature Distribution for a Friction Taper Stud Weld in Thick Walled 10CrMo910 Steel

Abstract

Heat distribution by direct measurement, as a function of weld time and position, during friction taper stud welding (FTSW) in 10CrMo910 thick wall steam pipe coupon is investigated. As expected, the main hotspots during welding were identified to be close to the top surface just before weld completion and at the bottom centre surface of the plug weld at the interface line. The maximum temperature of 1102 °C was recorded at the tool hole interface within 3 s after the start of the weld. This corresponds to the initial "dry friction " stage where the heat generation initiates due to friction between the tool and parent plate. The weld power calculated from motor torque increases rapidly at the start of the weld and reached a peak value after 8 s, while a temperature of 964 °C was reached after 34 s, at the top edge of the weld. This position of the second peak temperature are most probably the result of heat transferred together with the accumulation of expelled material forming on the surface of the parent plate during the FTSW process.

Thermocouple; heat transfer; solid state; thermal profile; forging; ferritic; creep resistant steel; third body


location_on
South African Institution of Mechanical Engineering Research and Development Journal, University of Stellenbosch, Private Bag X1, Matieland, Cape Town, Western Cape Province, ZA, 7602, Tel: +27 21 808 4091 - E-mail: gillianc@sun.ac.za
rss_feed Acompanhe os números deste periódico no seu leitor de RSS
Ir para o topo