Open-access Control of complex inclusions in high-strength ship plate steel by reducing calcium treatment

Abstract

To eliminate nozzle clogging during continuous casting of ship plate steel and reduce the calcium addition required, the composition of CaO-MgO-Al2O3 inclusions in the liquid phase region must be controlled. Thermodynamic calculations using FactSage show that when the balanced Al content is 0.03 mass %, aCain the liquid steel is 1-10 ppm, and aMgis 0.01-0.3 ppm; and when the balanced Al content is 0.06 mass %, aCa in the liquid steel is 1-30 ppm, and aMgis 0.05-0.9 ppm. The CaO-Al2O3-CaS inclusions can be controlled in the liquid region below 1600°C at aCavalues of 5 ppm, 15 ppm, and 30 ppm, and the balanced Al content should be controlled in the range of 0.001-0.050, 0.005-0.250, and 0.010-0.50 mass %, respectively. Based on theoretical analysis, the refining slag composition should be controlled to 45-53 mass % CaO, 30-37 mass % Al2O3, 6-12 mass % SiO2, and 6-8 mass % MgO. Optimization of the slag system and steel composition can reduce, or even eliminate, the requirement for calcium treatment. The total oxygen content in the slab can be controlled to 15-21 ppm, with typical micro-inclusions < 10 μm in size, with compositions in the CaO-Al2O3-MgO and CaO-Al2O3-CaS systems.

alcium treatment; refining slag; inclusions; ship plate steel; melting point


location_on
The Southern African Institute of Mining and Metallurgy The Southern African Institute of Mining and Metallurgy, 5 Hollard Street, P.O. Box 61127, Marshalltown, Johannesburg, Gauteng, ZA, 2107, Tel: +27 11 834 1273, Tel: +27 11 834 1277 - E-mail: journal@saimm.co.za
rss_feed Acompañe los números de esta revista en su lector de RSS
Ir para arriba